1. The short version: strong tinting strength means start small

Our selection guide puts it plainly: fluorescent pigments offer exceptional brilliance and very high color strength — a small amount dominates a formulation’s color. The products page says the same in short: bright colors, strong color strength. That is the advantage — and the matching problem.

So matching is not “add enough and be done”; it is add a little, look, then adjust in small steps. Add too much at once and correcting back is harder than moving forward; on a fluorescent colour, a small error shows more than on an ordinary pigment. The first rule of matching is: do not start heavy-handed.

2. What tinting strength is: dye in resin, brightness from fluorescence

A fluorescent pigment’s colour comes from a dye dissolved in resin — the dye is held inside the resin particle, forming a solid solution (the definition from Article 10). Its brightness comes from fluorescence: the dye turns part of the light the eye cannot see into visible light, which is why fluorescent colours look so bright in daylight.

Strong tinting strength means a given amount of dye carries a lot of colour. And that is the matching difficulty: the colour is not decided by how much was added alone, but by the dye itself, the resin, the substrate and the light together. Adjusting dosage alone will not get the colour right.

3. Series first, colour second

Before matching, choose the series by application (the guide’s application table and choose-by-application section): injection moulding looks at DX or DZ, water-based coatings list DX only, powder coatings look at DZ, DP or DFQ. Get the series wrong and the colour match is worthless — heat resistance, migration and compatibility are all series questions.

Colour availability also varies by series: the guide notes, for example, that sapphire blue and strong magenta exist only in DX. Before promising a colour, check that the target colour exists in the chosen series; if it does not, change the series or the target — do not force the match.

For masterbatch matching, look at DQ and DFQ first: these two series were developed for masterbatch, with strong colour strength and dispersibility and heat resistance designed for that use. Start with the series that fits the job, then talk colour.

4. Start from the closest single colour; change one thing at a time

Find the single colour closest to the target, then move toward the target in small steps. Do not start by blending three or four colours at once — every colour in the blend changes hue and brightness at the same time, and when the result is off, nobody knows which one caused it.

Keep a sample and a written record of the formula and conditions at every step; if a step goes wrong, you can go back to the previous one. A match with no record cannot be reproduced next time. Matching is not a feel for colour — it is being able to do it again.

5. More pigment is not more brightness

Past a point, adding more pigment stops making the colour proportionally brighter; the extra pigment brings three costs instead: cost, dispersion load, and migration risk. If dispersion is poor, adding more only adds undispersed material (the Article 10 rule); on migration, more pigment does not fix migration — more dye means more dye able to move (the Article 9 conclusion).

If the colour is not bright enough, check dispersion, series and substrate first, and only then consider dosage. This article gives no dosage figures: the right dosage depends on the base paint, the substrate and the colour, and must be set by trial.

6. Judge only the dry film, on the same substrate, under the same light

The Article 10 rule applies unchanged: wet and dry films are not comparable. Judge only the dry film — same substrate, same drawdown, same drying conditions, side by side with the reference sample under the same light.

And judge it in the final system: a sample made in the real base paint, the real resin and the real processing conditions is the colour the customer will actually receive. A colour matched only in a paste or a lab sample can still drift in full production.

Keep a reference sample: one per batch, marked with date, series and colour (the Article 9 and 10 habit), so there is something to compare against when a dispute comes up.

7. Light and lightfastness: match for the place the colour will live

Fluorescent brightness is judged in daylight; under a different light, the colour looks different. Match under the light the customer will actually use, not under one lamp only.

Lightfastness is the fluorescent pigment’s weak point: daylight fluorescent pigments are naturally less lightfast than ordinary pigments, and long outdoor exposure fades them (the guide and Article 1 on lightfastness). A colour for long outdoor use should not be set from an indoor sample; agree with the customer first on how it will look after outdoor use.

And do not confuse the two: fluorescent is not glow-in-the-dark (Article 8). When a customer says “the colour must be bright at night”, ask first whether they want a fluorescent bright colour in daylight or a phosphorescent effect that keeps glowing after the lights go out — they are different product directions.

The heat ceiling still applies: DX is rated up to 195 °C; other series are given here only as “per their own TDS”, with no figures. Past the limit, the dye is damaged and the brightness is lost before the coating ever sees daylight (see Article 7).

8. Frequently asked questions

Q1: The colour is not bright enough — just add more pigment?

Not necessarily. Check dispersion, series and substrate first — if dispersion is poor, more pigment only adds undispersed material, and more dye also raises the migration risk. Dosage is the last variable to move, and it moves in small steps, with a sample kept at each step for comparison.

Q2: The lab sample matched — why did production drift?

Because the system changed: base paint, substrate, dispersing equipment, drying conditions — any one of them can move the colour. A lab match is only step one; before fixing the colour, remake the sample under production conditions and compare it side by side with the reference sample. Keep the reference sample, so a production dispute has something to check against.

Q3: The customer just says “match this colour” — what do I ask first?

Ask three things: an effect or a specific shade, the application (which fixes the series), and the light and environment it will be used in (indoors or outdoors). Then ask for the TDS and confirm the target colour exists in the chosen series. Quoting before series, colour and environment are clear risks matching a colour the customer never wanted.

In short: fluorescent pigments tint strongly, so matching is won not by adding more, but by fixing the series first, starting from one colour, adjusting in small steps, and judging only the dry film.